MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Tecnoflon® N 535 Fluorelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Tecnoflon® N 535 is a low viscosity fluoroelastomer copolymer. Tecnoflon® N 535 is intended as a general purpose fluoroelastomer. It can be blended with other polymers of the Tecnoflon® family to meet specific requirements. Tecnoflon® N 535 does not contain curatives: therefore the proper levels of Tecnoflon® FOR M1 and Tecnoflon® FOR M2 must be added to achieve the required properties. It can be also cured with diamine based systems such as Tecnoflon® Tecnocin A and Tecnoflon® Tecnocin B.

Some of the unique properties of Tecnoflon® N 535 are:
- Excellent compression set
- Lack of mold fouling
- Superior extrusion behavior
- Superior mold flow
- Excellent mold release

Tecnoflon® N 535 can be used for injection and transfer molding of O-rings, gaskets and seals. The product can be mixed using typical fluoroelastomers compounding ingredients and mixing can be accomplished with two-roll mills or internal mixers. The material can be extruded into hoses or profiles and can be calendered to make sheet stocks or belting. Compounds based on Tecnoflon® N 535 can be dispersed in solvents for coating applications. Finished goods can be produced by a variety of rubber processing methods.

Applications: Belts/Belt Repair; Blending; Gaskets; General Purpose; Hose; Profiles; Seals; Sheet

Features: Copolymer; Good Flow; Good Mold Release; Low Compression Set; Low Viscosity

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 27
@Temperature 121 °C
27
@Temperature 250 °F
ML 1+10; ASTM D1646
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 66 %66 %
 
Descriptive Properties
AvailabilityEurope
 North America
ColorTranslucent
FormsSlab
ProcessingCalendering; Compounding
 Extrusion; Injection Molding; Resin Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4519 / 280319

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.