MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SK Chemicals SKYTHANE® SG200 SKYGREEN Biodegradable Thermoplastic  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganisms

SKYGREEN, biodegradable thermoplastics, has been developed on the basis of the SK Chemicals polyethylene terephthalate (PET) technology. There is no other chemical linkage than ester in its molecular structure.

SkyGreen fully degrades into CO2 and H2O via hydrolysis mechanism. Within 45 days, the polymer degrades completely in the composting condition.

Information provided by SK Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55ASTM D2240
Tensile Strength, Ultimate 220 kg(f)/cm²ASTM D638
Elongation at Break 400 %ASTM D638
Flexural Yield Strength 182 kg(f)/cm²ASTM D790
Flexural Modulus 2914 kg(f)/cm²ASTM D790
Izod Impact, Notched 30.0 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 90.0 °CASTM D3418
Softening Point 79.0 °CASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SK Chemicals SKYTHANE® SG100 SKYGREEN Biodegradable Thermoplastic
SK Chemicals SKYTHANE® SG400 SKYGREEN Biodegradable Thermoplastic
BASF Ecoflex® 1200 F Blend Biodegradable Polyester
Evonik DYNAPOL® S EP1408 Linear Copolyester
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin

PSK102 / 67834

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.