MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 299 X 150123 Nylon 6/6 (PA), Long Glass Fiber - Carbon Fiber - ESD Protection - Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Carbon Fiber Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D 792
Additive Loading 50 %Primary Additive
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 38000 psiASTM D 638
Elongation at Break 2.1 %ASTM D 638
Tensile Modulus 2900 ksiASTM D 638
Flexural Strength 56000 psiASTM D 790
Flexural Modulus 2600 ksiASTM D 790
Izod Impact, Notched 4.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 22.0 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.0 - 1000 ohm-cmASTM D 257
Surface Resistance 100 - 10000 ohmESD STM11.11
Surface Resistivity per Square 1000 ohm - 1e+05ASTM D 257; ESD STM11.11
Static Decay <= 0.50 secFTMS101C; 4046.1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 530 - 570 °F
Mold Temperature 150 - 225 °F
Drying Temperature 175 °F
@Time 14400 sec
Moisture Content 0.20 %
Dew Point 0.000 °F
Injection Pressure 10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company EMI 2561 FR UV Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant - UV Stabilized
RTP Company EMI 2562 UV BLACK Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized
RTP Company EMI 362 UV BLACK Polycarbonate (PC); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized
RTP Company ESD 187 Polypropylene (PP), Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company ESD 189 Polypropylene (PP), Carbon Fiber - Electrically Conductive - EMI/RFI/ESD Protection

PQZQA41231 / 239965

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.