MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Braskem FL105PP 3D Printing Polypropylene Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: FL105PP is a next generation polypropylene (PP) filament designed to provide superior dimensional accuracy, inherently low density, high fatigue, and high moisture resistance for use in Fused Filament Fabrication (FFF). Additionally, FL105PP provides a balance of impact resistance and dimensional accuracy while enabling the production of watertight, lightweight and chemically resistant parts.

Printed part properties obtained using test specimens printed in X-Y direction.

Information provided by Braskem.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 11.0 MPa1600 psiASTM D638
Elongation at Yield 17 %17 %ASTM D638
Modulus of Elasticity 1.02 GPa148 ksiASTM D638
Flexural Modulus 0.840 GPa122 ksiChord Modulus; ASTM D790
Charpy Impact, Notched 1.17 J/cm²5.57 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FASTM D648
Vicat Softening Point 130 °C266 °F10 N; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 220 - 230 °C428 - 446 °F
 
Descriptive Properties
Bed temperature (°C)20-40Multi-purpose adhesive spray
 60-80PP bed adhesion solution stick
Printing speed (mm/s)35-65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRAS693 / 291046

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.