MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® L2124 sw 9.7507 (dry properties) Nylon 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: Uses: Flexible tubing for the automobile industry.

ISO data as provided by the manufacturer.

Key Words: Polyamide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
Moisture Absorption at Equilibrium <= 0.50 %Humidity Absorption
Melt Flow 170 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 27.0 MPa
Elongation at Break >= 50 %
Elongation at Yield 29 %
Modulus of Elasticity 0.430 GPa
Charpy Impact Unnotched NB
 NB
@Temperature -30.0 °C
Charpy Impact, Notched NB
 0.600 J/cm²
@Temperature -30.0 °C
Tensile Creep Modulus, 1 hour 310 MPa
Tensile Creep Modulus, 1000 hours 290 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.00e+12 ohm-cm
Surface Resistance 5.00e+14 ohm
Dielectric Constant 3.0
@Frequency 1e+6 Hz
 13
@Frequency 100 Hz
Dielectric Strength 34.0 kV/mm
Dissipation Factor 0.13
@Frequency 1e+6 Hz
 0.15
@Frequency 100 Hz
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 20.0 °C
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
Vicat Softening Point 125 °C50°C/hr/50 N
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestamid® L2121 sw 9.7507 (dry properties) Nylon 12
Evonik Vestamid® L2122 sw 9.7507 (dry properties) Nylon 12
Evonik Vestamid® L2123 sw 9.7507 (dry properties) Nylon 12
Evonik Vestamid® L2121 sw 9.7507 (as-conditioned) Nylon 12
Evonik Vestamid® L2123 sw 9.7507 (as-conditioned) Nylon 12

PHUL77 / 47337

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.