MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm PLEXIGLAS® Film HC 0F028 PMMA  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Acrylic (PMMA)

Material Notes: Product: EUROPLEX® Film HC 0F028 is a weather resistant and transparent co-extruded PMMA and PVDF film. It is designed to bring a state of the art UV protection and surface finish for thermoset materials such as High Pressure Laminates. This film shows excellent performance in long term outdoor weathering without the risk of color change or yellowing. The PMMA layer is based on a tailor made PMMA resin that provides excellent chemical adhesion to melamine resin while the PVDF top layer brings a high level of weatherability as well as a very good chemical resistance, anti-soiling, anti-fouling and easy to clean properties including graffiti.

Application: Due to its very good chemical adhesion to melamine resin combined with its excellent UV and weather resistance, EUROPLEX® Film HC 0F028 is suitable to be used as top layer on panels of exterior grade compact laminates.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccDIN 53479
Surface Tension 23 dynes/cmPVDF; DIN 53364
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 44.0 MPaISO 527-3
Elongation at Break >= 50 %ISO 527-3
Elongation at Yield 7.0 %ISO 527-3
 
Optical PropertiesOriginal ValueComments
Haze 7.0 %ASTM D1003
Transmission, Visible >= 92 %ISO 13458-2
UV Transmittance <= 2.0 %
@Wavelength 280 - 380 nm
DIN EN 410

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucite International Elvacite® 2044 Acrylic Resin
Polycasa Acryl® KR 2007/1 Acrylic
Röhm Plexiglas® 99845 Crystal Clear Elastomer Based Film
Polycasa Acryl® KR 2014/1 Acrylic, Impact Grade
Evonik DEGALAN® P24 Methacrylic Polymer

PEVONIL030 / 196235

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.