MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® X7375 nf (dry properties) Polyether Block Amide (PEBA)  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyether Block Amide (PEBA)

Material Notes: Uses: Ski upper surfaces.

ISO data as provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/cc
Water Absorption 1.0 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 68
Tensile Strength, Yield 31.0 MPa
Elongation at Break >= 50 %
Elongation at Yield 19 %
Modulus of Elasticity 0.750 GPa
Charpy Impact Unnotched NB
 NB
@Temperature -30.0 °C
Charpy Impact, Notched 4.40 J/cm²
 0.700 J/cm²
@Temperature -30.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.00e+13 ohm-cm
Dielectric Constant 4.0
@Frequency 1e+6 Hz
 7.0
@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm
Dissipation Factor 0.076
@Frequency 1e+6 Hz
 0.15
@Frequency 100 Hz
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 20.0 °C
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
Vicat Softening Point 130 °C50°C/hr/50 N
Flammability, UL94 HB
@Thickness 1.60 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestamid® E40-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer
Evonik Vestamid® X4442 nf (dry properties) Polyether Block Amide (PEBA)
Arkema Pebax® MV 1041 SA 01 Polyether Block Amide (PEBA)
Evonik Vestamid® E50-R2 Heat & Light Stabilized Nylon 12/PEBA Elastomer
Evonik Vestamid® E47-S3 Heat & Light Stabilized Nylon 12/PEBA Elastomer

PHUL98 / 47358

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.