MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sinotek Materials MD-2 Graphite Emulsion
Categories: Carbon; Graphite; Fluid; Lubricant

Material Notes: The graphite emulsion is forged with patented equipment and a unique recipe. It is an ideal lubricant for high-temperature demolding in hot processing of non-ferrous metal. The superior products are used in aviation and space flight as well as extrusion of warheads and cartridge cases. With ideal high-temperature lubricity and cohesiveness, it makes demolding easy. It is chemically stable, non-corrosive and non-toxic. It can improve the moulding quality and remarkably prolong the life of moulds. Examples of application include drop forging, roll forging, gear rough and finish forge.

Information provided by Sinotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 28 %
 
Descriptive Properties
Graphite Content %24
Subsidency After 3 hrs, 20 Times of Dilution %35

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Milliken® Syn Fac 334-13 Dispersant
Sinotek Materials MD-6 Graphite Emulsion
Dow 5 Compound
Dow UCON™ 50-HB-3520 PAG Lubricant
Goodfellow CVD Graphene Film on Quartz Glass

CSINOT56 / 2113

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.