MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allvac® 330 UNS N08330 Nickel Superalloy  (discontinued **)
Categories: Metal; Superalloy; Iron Base

Material Notes: Uses: Weld wire, woven wire mesh belts, rod for heat treat baskets, heat treat fixtures.

Property values are for samples in the metallurgical condition: As rolled.

Information provided by Allvac, An Allegheny Teledyne Company.

Key Words: AMS 5592, 5716. ASTM B 511, B 512, B 535, B 536, B 739.
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 80
Tensile Strength, Ultimate 586 MPa
Tensile Strength, Yield 276 MPa
@Strain 0.2 %
Elongation at Break 40 %
Reduction of Area 70 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.040 %
Chromium, Cr 18.5 %
Copper, Cu 0.50 %
Iron, Fe 43 %as balance
Lead, Pb 0.0010 %
Manganese, Mn 1.0 %
Nickel, Ni 35.5 %
Phosphorus, P 0.010 %
Silicon, Si 1.13 %
Sulfur, S 0.010 %
Tin, Sn 0.010 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cunife® Hard Magnetic Alloy
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested longitudinal, round bar 75 mm
ATI Allvac® 706 Nickel Superalloy, Heat Treatment: 954°C (1750°F) + Age
ATI Allvac® Nickelvac® 825 UNS N08825 Nickel Superalloy
ATI Allvac® Nickelvac® 601 UNS N06601 Nickel Superalloy

NALLV09 / 14925

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.