MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 2599 X 131264 C Polycarbonate/ABS Alloy (PC/ABS), Fiber Reinforced - Electrically Conductive - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Antistat/Conductive; Polycarbonate (PC)

Material Notes: Preliminary Data Sheet

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D 792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 13000 psiASTM D 638
Elongation at Break 1.0 - 2.0 %ASTM D 638
Tensile Modulus 1800 ksiASTM D 638
Flexural Strength 21000 psiASTM D 790
Flexural Modulus 1500 ksiASTM D 790
Izod Impact, Notched 1.40 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 8.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.0 ohm-cmASTM D 257
Surface Resistance <= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness 73 dB
@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
ASTM D 4935
 75 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 75 dB
@Thickness 3.00 mm,
Frequency 1.50e+8 Hz
ASTM D 4935
 79 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 81 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 82 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 82 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 83 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 250 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 470 - 525 °F
Mold Temperature 125 - 200 °F
Drying Temperature 200 °F
@Time 14400 sec
Moisture Content 0.020 %
Dew Point -20.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company EMI 2185  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 30%
RTP Company EMI 2184  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 25%
RTP Company EMI 2183  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 20%
RTP Company EMI 2162 Polyetherimide (PEI); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1382  Polyphenylene Sulfide (PPS) Shielding - Nickel-Coated Carbon Fiber 15%

PQZTA26243 / 159250

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.