Combines the processing ease of conventional thermoplastic resins with the excellent properties of PTFE. High chemical resistance, superior electrical properties, high service temperatures, superior high temperature creep resistance, excellent low temperature toughness, and exceptional flame resistance. Processed by conventional melt-extrusion and molding techniques. Resin Characteristics: General purpose; highest flow rate. Uses: Tubing; injection- or blow-molded articlesChemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015. This specific product was discontinued prior to the formation of Chemours. |