MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

American Elements Calcium Oxide Nanopowder
Categories: Ceramic; Oxide

Material Notes: General Description

Calcium Oxide ( CaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Calcium Oxide Particles are typically 20-80 nanometers (nm) with specific surface area (SSA) in the 15 – 50 m 2 /g range and also available in with an average particle size of 100 nm range with a specific surface area of approximately 5 - 10 m 2 /g. Nano Calcium Oxide Particles are also available in ultra high purity and high purity, transparent, and coated and dispersed forms. Applications for Calcium Oxide Nanocrystals include as a possible flame retardant and in the clean up of toxic contamination from chemical warfare. Calcium Oxide Nano Particles are generally immediately available in most volumes.

Key Words: Formula: CaO; CAS Number: 1305-78-8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.020 - 0.080 µm0.020 - 0.080 µm
 0.10 µm0.10 µm
Specific Surface Area 5.0 - 10 m²/g5.0 - 10 m²/g
 15 - 50 m²/g15 - 50 m²/g
Molecular Weight 56.08 g/mol56.08 g/mol
 
Descriptive Properties
AppearanceWhite Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Viton® GFLT-600S with CaO Fluoroelastomer Compound
Calcium Oxide, CaO

EJAMER16 / 5499

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.