MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Master Bond MasterSil 912Med Silicone
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Key Features:
  • Meets USP Class VI requirements
  • Passes ISO 10993-5 testing
  • Fast curing
  • Paste consistency
  • Excellent performance profile
  • Good sterilization resistance
Product Description: MasterSil 912Med is a specially formulated RTV silicone system for bonding, sealing and coating primarily for medical devices. It is a non-corrosive, neutral type curing system with a paste viscosity. It passes both USP Class VI testing and ISO cytotoxicity standards. Upon curing, it bonds well to a wide variety of substrates, including metals, composites, ceramics, glass as well as many rubbers and plastics. MasterSil 912Med can withstand highly rigorous thermal cycling as well as thermal and mechanical shock. Similar to other one part silicones, the curing mechanism is based on the humidity level. The higher the humidity, the faster the cure and thinner sections cure more quickly than thicker ones. MasterSil 912Med is a faster curing system with a tack free time of 15-30 minutes, depending upon the variables mentioned previously. It resists many kinds of sterilization including gamma and other types of radiation, EtO and some types of liquid sterilants. The service temperature range extends from -75°F to +400°F. One particularly useful product property is its ability to adhere well to silicone substrates. MasterSil 912Med can be used in a wide array of medical device applications where the unique properties of a silicone are desirable. It should be emphasized that for biocompatibility testing, a full cure of at least 7 days is recommended.

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30 - 4030 - 40
Tensile Strength 4.83 - 7.58 MPa700 - 1100 psi
Elongation at Break 250 - 350 %250 - 350 %
Adhesive Bond Strength 1.38 - 2.07 MPa200 - 300 psiTensile Lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 2.8
@Frequency 60 Hz
2.8
@Frequency 60 Hz
Dissipation Factor 0.0030
@Frequency 60 Hz
0.0030
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -59.4 °C-75.0 °F
 
Processing PropertiesMetricEnglishComments
Tack-Free Time 15.0 - 30.0 min0.250 - 0.500 hour
Shelf Life 6.00 Month
@Temperature <=23.9 °C
6.00 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
Colortranslucent
Viscositypaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials Silopren™ LSR 4630 FC Liquid Silicone Rubber - Healthcare
Momentive Performance Materials Silopren™ LSR 2630 Liquid Silicone Rubber - Fast Cure / High Tear

PMASTM939 / 185532

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.