MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Recommended for interior applications.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 6715 sec; ASTM D2240
 75ASTM D2240
Tensile Strength at Break 12.4 MPa510 mm/min; ASTM D638
Tensile Stress at Strain 5.03 MPa
@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 420 %510 mm/min; ASTM D638
Tear Strength 49.0 kN/mDie C, 510 mm/min; ASTM D624
Compression Set 30 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395
Clash Berg Modulus 98.6 MPaASTM D1043
 310 MPa
@Temperature -47.0 °C
ASTM D1043
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -46.7 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 174 - 179 °C
 193 - 204 °C
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesGeneral Purpose
 Low Gloss
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesGeneral Purpose

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Flexible D8000 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible P484 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible R8180K Polyvinyl Chloride, Flexible
Geon® Performance Solutions SF M7000 Polyvinyl Chloride, Rigid
Geon® Performance Solutions HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy)

PH0POL0067 / 144636

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.