MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics THERM-A-GAP™ G574 Highly Conformable and Thermally Conductive Elastomer
Categories: Ceramic; Polymer; Thermoset; Silicone

Material Notes: Description: THERM-A-GAP™ elastomers are used to fill air gaps between PC boards or other components and heat sinks, metal enclosures, and chassis. The exceptional conformability of these advanced materials enables them to blanket highly uneven surfaces, transferring heat away from individual components or entire boards, and allowing chassis parts to be used as heat spreaders where space is restricted. The 574 thermal interface pads provide superior thermal performance and are softer than other THERM-A-GAP™ materials. G574 material consists of an extremely soft silicone elastomer loaded with ceramic particles, coated onto a fiberglass cattier. The “G” designates the fiberglass cattier that is on one side of the material. This reinforces the pad and makes one side of the pad non-tacky. The non-tacky side can be easily removed for component repairs. The flexible, elastic nature allows the material to blanket highly uneven surfaces, drawing away and transferring heat from components such as microprocessors, video chips, and power devices. These fiberglass-reinforced pads consist of an electrically non-conductive ceramic filled silicone elastomer with a thermal conductivity of 1.6 W/m-K. These pads are best suited for applications where a gap of approximately .040 to 0.200 inch needs to be filled under pressures of 5 to 20 psi.

Application: G574 is inherently self-adhering on the side opposite from the fiberglass carrier for ease of pad application. Remove the liner and place pad on the desire heat pipe or a microprocessor heat sink. The pads can be removed from the fiberglass side (non-tacky side) for rework.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/ccASTM D792
Thickness 1000 - 5100 micronsASTM D374
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A <= 5.0ASTM D2240
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.60 W/m-KASTM D5470
 
Descriptive Properties
CarrierFiberglass
ColorLight Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Superior Flux Superior AL261-143-75 Direct Aluminum Solder Paste

PCHOME321 / 131031

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.