MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Materion SupremEX® 225XE Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Billet  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: SupremEX® 225XE is a high quality aerospace grade aluminum alloy (AA2124) that offers a high tensile modulus approximately 60 percent higher than the parent alloy and slightly higher than that of titanium. It also offers good strength, excellent fatigue characteristics and is particularly well suited for applications demanding a good balance of properties.

CWQ = Cold Water Quench

Information supplied by Materion.

Key Words: AlSiC. Designation: – 2124/SiC/25p
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.88 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 82.7 ksi
Tensile Strength, Yield 68.2 ksi
@Strain 0.2 %
Elongation at Break 1.8 %
Modulus of Elasticity 115 GPa
Poissons Ratio 0.30
Shear Modulus 44.2 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.1 µm/m-°C
Specific Heat Capacity 0.848 J/g-°C
Thermal Conductivity 150 W/m-K
Melting Point >= 548 °C
Solidus 548 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion SupremEX® 217XG Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Billet
Aluminum - SiC Metal Matrix Composite
Materion SupremEX® 217XG Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Forged Plate
Materion SupremEX® 217XG Aluminum - Silicon Carbide Metal Matrix Composite, T6 PGQ Billet
Materion SupremEX® 225XE Aluminum - Silicon Carbide Metal Matrix Composite, T6 HWQ Billet

NBB9105 / 192326

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.