SARAN WRAP™ 18 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for chub packaging machines and laminations. It is available in 100 gauge, as single or double would rolls, in widths up to 60 inches.Dow has sold the Saran Wrap product line. |