MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Stat-Tech™ ST5220-0004 CP4D EG Black Polypropylene Impact Copolymer (PP Impact Copolymer)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low-to-high levels of conductivity depending upon application requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.948 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.020 cm/cmASTM D955
Melt Flow 0.52 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 17.2 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 38 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 1070 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 37.2 MPaASTM D790
Flexural Modulus 1100 MPaASTM D790
Izod Impact, Notched 230 J/m
@Thickness 6.35 mm,
Temperature 23.0 °C
Injection Molded, Method A, 1200 mm Notch Depth; ASTM D648
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.20e+6 ohm-cmASTM D257
Surface Resistance 760000 ohmASTM D257
 
Descriptive Properties
AppearanceBlack
FeaturesElectrically Conductive
 High Flow
FormsPellets
Generic MaterialPP Impact Copolymer
Generic NamePolypropylene Impact Copolymer (PP Impact Copolymer)
Processing MethodExtrusion
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Industrial Applications
 Medical/Healthcare Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unipetrol PP MONSTEN® MB 720 Polypropylene Impact Copolymer
RTP Company RTP 199 X 123298 B Polypropylene (PP) ESD Protection - Permanently Static Dissipative - Impact Modified - UV Stabilized
RTP Company RTP 199 X 141363 A Polypropylene (PP); TPO (Thermoplastic Polyolefin) - ESD Protection - Permanently Static Dissipative - Impact Modified - Mineral - Preliminary
RTP Company RTP 199 X 144660 Polypropylene (PP); ESD Protection - Permanently Static Dissipative - Impact Modified - UV Stabilized - Preliminary Datasheet
Unipetrol PP MONSTEN® MA 611 Polypropylene Impact Copolymer

PH0POL1424 / 145993

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.