Kraton DX421 J is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 16% mass. It is supplied from Japan. Kraton DX421 J is used in formulating adhesives, sealants and coatings. It is also used as a modifier of bitumen and polymers and in formulating compounds. Kraton DX421 JSP supplied as dusted, dense pellet. Information provided by Kraton Corporation. |