MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Titanium Grade 11
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Same composition as Grade 7 except impurity limits. 0.2% Pd added for corrosion resistance, very effective for improving crevice corrosion at elevated temperatures and where in contact with mildly reducing or variable oxidizing-reducing media. Properties are very similar to Ti Grade 1 because the addition of small amount of Pd does not significantly change microstructure.

Applications: Chemical processing and storage - containers, heat exchangers, ducting, pumps, valves, fittings and auxiliary equipment.

Forms typically available: billet, bar, plate, sheet, strip, rod, wire, extrusions, tubing.

Titanium Grades 1,2,3,4,7,11,and 12 are all considered unalloyed and have similar mechanical properties.

Key Words: ASTM Grade 11; UNS R52250, CP titanium, C.P. titanium alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 240 MPa
Tensile Strength, Yield 170 - 310 MPa
Elongation at Break 24 %
Tensile Modulus 105 GPa
Compressive Modulus 110 GPa
Poissons Ratio 0.37
Shear Modulus 45.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000550 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 325 J/gHigh Purity Ti.
CTE, linear 8.60 µm/m-°C
@Temperature 0.000 - 100 °C
 9.20 µm/m-°C
@Temperature 0.000 - 315 °C
average
 9.70 µm/m-°C
@Temperature 0.000 - 540 °C
perpendicular to the c-axis
Specific Heat Capacity 0.523 J/g-°C
@Temperature 23.0 °C
 0.670 J/g-°C
@Temperature 540 °C
Thermal Conductivity 17.0 W/m-Kestimated from other grades of unalloyed Ti
Melting Point <= 1670 °C
Liquidus 1670 °C
Maximum Service Temperature, Air 425 °CContinuous use
 540 °CIntermittent Use
Beta Transus 888 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.30
@Temperature 710 °C
High purity Ti
Reflection Coefficient, Visible (0-1) 0.56High purity Ti; visible light.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.080 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.20 %
Nitrogen, N <= 0.030 %
Other, each <= 0.050 %
Other, total <= 0.30 %
Oxygen, O <= 0.20 %
Palladium, Pd 0.12 - 0.25 %
Titanium, Ti 98.925 - 99.88 %As Balance; Elemental Composition per ASTM B265

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Grade 7
Titanium Grade 12
Titanium Grade 2
Titanium Grade 4
Titanium Grade 3

MTU110 / 14267

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.