MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schunk SiC30 Silicon Carbide/Graphite Composite
Categories: Ceramic; Ceramic Matrix Composite

Material Notes: Applications: The main fields of application of the SiC30 material are sliding rings and bearings for use in media with a poor lubricating capacity. The combination of excellent properties of graphite (good emergency-running properties, thermal shock resistance, etc.) and silicon carbide (hardness, strength, abrasion resistance) combined with an exceptional structure allows solving problems that would not be possible with other materials. The best results are often achieved with the material pairing of SiC30 to SiC30.

The material is resistant to:

  • aqueous salt solutions
  • organic reagents
  • strong acids (HF, HCl, H2SO4, HNO3)
  • hot inert gases

Information provided by Schunk Graphite Technology, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.65 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 140 GPa
Flexural Strength 140 MPa
Compressive Strength 500 MPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.00 µm/m-°C
@Temperature 20.0 - 200 °C
 4.00 µm/m-°C
@Temperature 200 - 600 °C
Thermal Conductivity 125 W/m-K
 
Component Elements PropertiesOriginal ValueComments
SiC 53 %
Silicon, Si 4.0 %
 
Descriptive Properties
Graphite43
HardnessConsists of a hard SiC- and a soft graphite phase
Inert Atmosphere2300°C
Oxidizing Atmosphere500°C
Spec. Electr. Resistance120 µOm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB
Schunk CarSIK CT Silicon Carbide
Schunk CarSIK NT Silicon Carbide
Schunk CarSIK SD Silicon Carbide
Silicon Carbide, Reaction-Bonded, SiSiC

CSCHU001 / 194758

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.