MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kumho-Sunny HEC0245 PC/AES
Categories: Polymer; Thermoplastic; AES Polymer; Polycarbonate (PC)

Material Notes: HEC0245 is high flow, non-halogen flame retardant PC/AES resin. HEC0245 has high flow properties and heat resistance. HEC0245 is mainly used in thin-wall product, automobile parts, etc.

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 20 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 53.0 MPaASTM D638
Elongation at Break 60 %ASTM D638
Flexural Strength 70.0 MPaASTM D790
Flexural Modulus 1900 MPaASTM D790
Izod Impact, Notched 500 J/m
@Thickness 3.20 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 265 °C
Mold Temperature 50.0 - 80.0 °C
Drying Temperature 90.0 - 100 °C
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKMSN146 / 280998

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.