MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Raschig Group EPOXIDUR® 3580 EP Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler; Filled/Reinforced Thermoset

Material Notes: Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS).

Processing: Injection and compression molding

Primary application: Electrical parts

Information provided by the Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.90 - 2.00 g/ccISO 1183
Apparent Bulk Density 0.600 - 0.900 g/ccISO 60
Water Absorption <= 0.10 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm(longitudinal) Injection and Compression; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 30.0 - 50.0 MPaInjection and Compression; ISO 527
Modulus of Elasticity 14.0 - 16.0 GPaInjection and Compression; ISO 527
Flexural Strength 70.0 - 100 MPaInjection and Compression; ISO 178
Flexural Modulus 17.0 - 20.0 GPaInjection and Compression; ISO 178
Compressive Strength 150 - 180 MPaISO 604
Charpy Impact Unnotched 0.400 - 0.600 J/cm²
@Temperature 23.0 °C
Injection and Compression; ISO 179/ 1eU
Charpy Impact, Notched 0.200 - 0.400 J/cm²
@Temperature 23.0 °C
Injection and Compression; ISO 179/ 1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 - 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 - 1.00e+15 ohmIEC 60093
Dielectric Constant 4.0 - 6.0
@Frequency 1e+6 Hz
IEC 60250
 5.0 - 7.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 30.0 - 40.0 kV/mmIEC 60243-1
Dissipation Factor 0.010 - 0.030
@Frequency 1e+6 Hz
IEC 60250
 0.030 - 0.050
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index >= 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C
@Temperature 50.0 - 150 °C
ISO 11359-2
Thermal Conductivity 0.400 - 0.600 W/m-KASTM E1461
Maximum Service Temperature, Air 180 °C
@Time 7.20e+7 sec
IEC 60216/T1
 240 °C
@Time <=180000 sec
IEC 60216/T1
Deflection Temperature at 0.46 MPa (66 psi) >= 200 °CInjection; ISO 75-B
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CInjection and Compression; ISO 75-A
Deflection Temperature at 8.0 MPa 180 - 200 °CInjection and Compression; ISO 75-C
Flammability, UL94 HB
@Thickness 1.60 mm
 V-0
@Thickness 6.00 mm
Shrinkage <= 0.050 %
@Temperature 110 °C,
Time 605000 sec
ISO 2577
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature <=20.0 °C
 
Descriptive Properties
Arc resistance4 StufeASTM D495
Glow wire flammability test900/1IEC 60695 2-12
Glow wire ignitability test900/1IEC 60695 2-13
Water Absorption<10 mg24h/23°C; ISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Raschig Group 3592 Epoxy
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade
Cookson Group Plaskon® 435 Mineral Filled Epoxy Molding Compound
Sumitomo Bakelite North America Epiall® 2061B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Aremco Aremco-Bond™ 526N High Performance Epoxide

PRASCH18 / 65303

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.