Description of Product: This specification covers wrought forging billets of molybdenum + 30% tungsten alloy produced from ingots consolidated by the H.C. Starck consumable electrode vacuum-arc-casting process. Structure: The billets will be supplied in the recrystallized condition, with a maximum hardness of 200 B.H.N. (10 mm ball/1500 kg/30 sec.). Material can also be supplied in the stress-relieved condition. Information provided by H.C. Starck. Elmet Technologies Acquired H.C. Starck Solutions Americas in 2023. |
Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.comClick here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |