MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
303 SE Stainless Steel, cold drawn, bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Key Words: T303, T 303, 303Se, 303SS, 303 SS, UNS S30323, AMS 5640 (type 2), AMS 5641, AMS 5738, ASME SA194, ASME SA320, ASTM A194, ASTM A194 (8F), ASTM A314, ASTM A320, ASTM A473, ASTM A581, ASTM A582, MIL SPEC MIL-S-862, SAE J405 (30303 Se), DIN 1.4305, X12CrNiS188, B.S. 303 S 41, EN 58M, , austenitic, 18-8
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 228
Hardness, Knoop 251Converted from Brinell
Hardness, Rockwell B 96Converted from Brinell
Hardness, Rockwell C 19Converted from Brinell hardness. Value below normal HRC range, for comparison only.
Hardness, Vickers 240Converted from Brinell
Tensile Strength, Ultimate 690 MPa
Tensile Strength, Yield 415 MPa
@Strain 0.2 %
Elongation at Break 40 %in 50 mm
Tensile Modulus 193 GPa
Poissons Ratio 0.25Calculated
Shear Modulus 77.2 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000720 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.2 µm/m-°C
@Temperature 0.000 - 100 °C
 17.8 µm/m-°C
@Temperature 0.000 - 315 °C
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.2 W/m-K
@Temperature 100 °C
 21.5 W/m-K
@Temperature 500 °C
Melting Point 1400 - 1420 °C
Solidus 1400 °C
Liquidus 1420 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 18 %
Iron, Fe 69 %
Manganese, Mn <= 2.0 %
Nickel, Ni 9.0 %
Phosphorus, P <= 0.20 %
Selenium, Se <= 0.15 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.060 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
303 Stainless Steel, cold drawn bar
303 Stainless Steel, annealed
304 Stainless Steel (UNS S30400); Annealed and Cold Worked Bar, 5/8" (16 mm) Diameter
303 SE Stainless Steel, annealed
303 SE Stainless Steel, annealed, bar

MQ303P / 12671

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.