MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond EP45HTND-2 Chemically Resistant, Non-Drip Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond EP45HTND-2 is a two component epoxy system for high performance bonding, sealing and coating. It is used for applications requiring solid temperature resistance and capable of withstanding aggressive chemicals. In fact, it is formulated to resist many of these chemicals even at elevated temperatures. EP45HTND-2 has a 100 to 30 mix ratio by weight. It contains no solvents or diluents, has a very smooth paste-like consistency as well as a very long open time. The system requires oven curing at 250-300°F for 3-4 hours. The optimal cure schedule is more of a ramp up type cure, that being 30-60 minutes at 200°F, 1 hour at 250°F and 2-3 hours at 300°F, followed by a post cure of 1-2 hours at 350°F. EP45HTND-2 will not flow or run when curing. It bonds well to metals, glass, ceramics, rubber and many plastics. The service temperature range is -80°F to +500°F. It is especially effective against aggressive chemicals particularly those found in downhole applications as well as many potent acids, bases and solvents. It is an outstanding electrical insulator with excellent physical strength properties. Both Parts A and B are colored amber. This versatile system is widely used in oil well, aerospace, electronic, specialty OEM and related applications where the cured properties mentioned above are needed and the material will stay in place while curing.

Product Advantages:

  • Easy to apply; paste viscosity; spreads evenly and smoothly.
  • Exceptionally long working life at room temperature.
  • Outstanding adhesion to a wide variety of substrates.
  • Highly resistant to many chemicals especially those in petroleum products.
  • Remarkable temperature resistance from -80°F to +500°F.
  • Fine physical strength property profile.
Key Features:
  • Non-drip paste consistency
  • Will not flow when curing
  • Outstanding chemical resistance
  • Serviceable from -80°F to +500°F

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  >= 70
@Temperature 149 °C
>= 70
@Temperature 300 °F
 >= 85
@Temperature 23.9 °C
>= 85
@Temperature 75.0 °F
Tensile Strength at Break >= 82.7 MPa>= 12000 psi
Tensile Modulus 3.10 GPa450 ksi
Shear Strength >= 17.2 MPa>= 2500 psiTensile lap, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 4.3
@Frequency 60 Hz,
Temperature 25.0 °C
4.3
@Frequency 60 Hz,
Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 - 40.0 µm/m-°C19.4 - 22.2 µin/in-°F
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
Glass Transition Temp, Tg >= 185 °C>= 365 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 - 60.0 min
@Temperature 93.3 °C
0.500 - 1.00 hour
@Temperature 200 °F
1 hour at 250°F and 2-3 hours at 300°F, plus a post cure of 1-2 hours at 350°F
 180 - 240 min
@Temperature 121 - 149 °C
3.00 - 4.00 hour
@Temperature 250 - 300 °F
Pot Life 720 - 1440 min720 - 1440 min100 gram batch
Shelf Life 12.0 Month12.0 Monthin original, unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)100:30by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resin Technology Group EN 239-2 Cationic UV Cure Epoxy Adhesive
Master Bond EP17HT-3 One component, snap-curing epoxy system
Atom Adhesives AA-BOND F253 Epoxy Adhesive
Atom Adhesives AA-BOND F112 Epoxy Adhesive

PMASTB404 / 149651

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.