MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe DuraTech™ Xtreme Powder Metal Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; Medium Carbon Steel; Tool Steel

Material Notes: DuraTech Xtreme tool steel is a medium-carbon, powder metallurgy tool steel which has an outstanding combination of properties including very high impact toughness, very good hot hardness, and good wear resistance. The impact toughness is enhanced by the fine grain size, small carbides, and superior cleanliness of the powder metallurgy (PM) microstructure. Typically, when selecting a tool steel, one must choose between high strength or high toughness, with a compromise in the other of these two properties. However, with an attainable hardness in the low 60s Rockwell C, the unique properties of DuraTech Xtreme make it an excellent choice for tooling applications which require both high strength and high impact toughness, heat resistance, or all of the above. DuraTech Xtreme should be considered for the most extreme service in blanking dies, sizing dies, shear blades, cold and hot forging punches, forging dies, gear rolling dies, and many other applications where a combination of strength and toughness

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.80 g/cc
Density 0.282 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 61.5Oil Quenched from 1066°C; 30 minutes
 63.5Oil Quenched from 1093°C; 15 minutes
Modulus of Elasticity 30000 ksi
Machinability 65 - 70 %1% Carbon Steel
Izod Impact Unnotched 70.0 ft-lbOil Quenched from 1080°C
 125 ft-lbOil Quenched from 1080°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.97 µm/m-°C
@Temperature 38.0 - 427 °C
 12.71 µm/m-°C
@Temperature 38.0 - 649 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.55 %
Chromium, Cr 4.0 %
Iron, Fe 88.79 %
Manganese, Mn 0.40 %
Molybdenum, Mo 4.25 %
Nickel, Ni 0.50 %
Silicon, Si 0.50 %
Sulfur, S 0.010 %
Vanadium, V 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Osprey S2 Tool Steel Powder (Grade 80% - 22)
Kinetics MIM 4605 Low Alloy Steel (Quenched + Tempered)
Sandvik Osprey 4340 Low Alloy Steel Powder (Grade 95% - 16)
Sandvik Osprey S2 Tool Steel Powder (Grade 95% - 16)
Excalibar ExCal® CW 100 Calcium Carbonate CaCO3 Powder

NTIMK127 / 19474

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.