MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Manufacturing Americas EZPrene 9070A TPV
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes:

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  69
@Time 5.00 sec
69
@Time 0.00139 hour
Extruded; ASTM D2240
 71
@Time 5.00 sec
71
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 6.10 MPa885 psiASTM D412
Elongation at Break 560 %560 %ASTM D412
100% Modulus 2.80 MPa
@Strain 100 %
406 psi
@Strain 100 %
ASTM D412
Tear Strength 31.0 kN/m177 pliASTM D624
Compression Set  34 %
@Temperature 23.0 °C,
Time 79200 sec
34 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
 46 %
@Temperature 125 °C,
Time 252000 sec
46 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
 
Descriptive Properties
Ozone ResistanceExcellentASTM D1149

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 201-67W171 Thermoplastic Vulcanizate Elastomer
Termopol Termoton® V2GA1065A TPV Compound
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer

PRAVAGO2010 / 221960

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.