HDPE K44-06-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as having a pipe material designation code of PE 3408, NSF Standard 14 certification, and compiles with ANSI/NSF Standard 61 health effects requirements. The hydrostatic design basis is 1600 psi at 23°C or 1000 psi at 60°C, based on ASTM test number D 2837. According to ASTM F 1473, the notch tensile (PENT) is greater than 100 hours. The cell classification is 345464A (ASTM D3350). |
Extrusion of potable water, industrial, and mining pipe |