MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sawbones Fourth-Generation Simulated Cancellous Bone (Rigid Polyurethane Bone)
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Glass Filled

Material Notes: Fourth-generation bones model natural cortical bone using a mixture of short glass fibers and epoxy resin pressure injected around a foam core. Standard bone models are manufactured with a solid rigid polyurethane foam cancellous core material, unless cellular rigid polyurethane foam is specified. The mid-shaft area has an intermedullarly canal.

Fourth-Generation Composite Bones Have Improved Properties

Fourth-generation composite cortical bone has been developed in order to meet the demanding needs of in vitro experiments, fatigue testing and to more closely simulate natural cortical bone. The result is a composite bone with enhancements to the following properties:

  • Fracture Toughness - Fatigue Crack Resistance
  • Fatigue Life - Implant Subsidence
  • Tensile Strength & Modulus - Compressive Strength & Modulus
  • Thermal Stability - Moisture Resistance
No changes have been made to the anatomical structure of the bones.

Information provided by Sawbones.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.270 g/ccSolid
 0.320 g/ccCellular
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 5.40 MPaCellular; ASTM D1621
 6.00 MPaSolid; ASTM D1621
Compressive Modulus 0.137 GPaCellular; ASTM D1621
 0.155 GPaSolid; ASTM D1621
Poissons Ratio 0.30ASTM D1621

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sawbones Fourth-Generation Simulated Cortical Bone (Short Fiber Filled Epoxy)
Sawbones Second-Generation Simulated Cancellous Bone (Solid)
Sawbones Third-Generation Simulated Cancellous Bone (Solid)
Sawbones Third-Generation Simulated Cancellous Bone (Cellular)
Sawbones Laminated Test Blocks

PSAWBO20 / 146109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.