MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastics Group Polifil® GFPP-10 10% Glass-Reinforced Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Glass Fiber Filler

Material Notes: Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuous temperature. Other benefits include reduced distortion under long-term stress.

Applications:

  • Appliances
  • Electrical components
  • Automotive
  • Utility products

Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccASTM D792
Density 0.980 g/ccASTM D792
Filler Content 10 %ASTM D2584
 10.0 %TPG WI
Water Absorption 0.000 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
@Thickness 1.59 mm
ASTM D955
 0.00500 in/in
@Thickness 3.17 mm
ASTM D955
Melt Flow 8.0 - 12 g/10 min230/2.16; May be specified; ASTM D1238
 4.00 - 10.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 85.0ASTM D785
Tensile Strength at Break 5700 psiASTM D638
Tensile Strength 5700 psiASTM D638
Elongation at Break 6.00 %ASTM D638
Elongation at Yield 3.00 %ASTM D638
Tensile Modulus 295 ksiASTM D638
Flexural Strength 7400 psiASTM D638
 7400 psiASTM D790
Flexural Modulus 340 ksitangent; ASTM D790
 340000 psiTangent; ASTM D790
Izod Impact, Notched 1.00 ft-lb/inAt 73°F; ASTM D256
 1.00 ft-lb/inASTM D256
Gardner Impact 0.667 ft-lbASTM D3029
 8.00 in-lb
@Thickness 12.7 mm
tup; ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 275 °FASTM D648
 285 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 255 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 410 - 430 °F
Middle Barrel Temperature 420 - 440 °F
Front Barrel Temperature 440 - 460 °F
Nozzle Temperature 440 - 480 °F
Melt Temperature 450 - 500 °F
Mold Temperature 120 - 150 °F
Drying Temperature 180 - 220 °C
@Time 3600 - 7200 sec
Back Pressure 25.0 - 75.0 psi
Screw Speed 30.0 - 60.0 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastics Group Polifil® GFPP-20 20% Glass-Reinforced Polypropylene
Overview of materials for Polypropylene with 10% Glass Fiber Filler
Plastcom SLOVALEN PC 51 GF 10 PP, 10% glass fibre
LG Chemical LUPOL GP2100 PP+GF10%
ExxonMobil SpectraSyn™ 100 Polyalphaolefin (PAO) Fluid

PPOLI023 / 56927

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.