MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Kanthal 200 Thermostatic bimetal
Categories: Metal; Superalloy; Iron Base

Material Notes: KANTHAL 200 is a thermostatic bimetal which is recommended for use in the temperature range -20 to +250°C.

Typical applications for KANTHAL 200 are in circuit breakers, motor protection units, thermostats, shower mixers etc.

High-expansive component: 72-18-10 Alloy(411 Designation, 53.9% of thickness)

Low-expansive component: Invar 155 Alloy (450 Designation, 46.1% of thickness)

Information provided by Sandvik

Composition:

  • High-expansive component: Designation 410; 74% Mn; 24.5% Ni; 1% Cu
  • Low-expansive component: Designation 450; 0.12% Mn; 36.8% Ni; Bal. Fe
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 120120High-expansive component
 130130Low-expansive component
 210210Low-expansive component, Cold-worked 20%
 230230High-expansive component, Cold-worked 20%
Tensile Strength, Ultimate 450 MPa65300 psiLow-expansive component
 540 MPa78300 psiHigh-expansive component
Tensile Strength, Yield 260 MPa37700 psiHigh-expansive component
 290 MPa42100 psiLow-expansive component
Elongation at Break 40 %40 %Low-expansive component
 50 %50 %High-expansive component
Modulus of Elasticity 135 GPa19600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.000109 ohm-cm
@Temperature 0.000 °C
0.000109 ohm-cm
@Temperature 32.0 °F
Bimetal
 0.000127 ohm-cm
@Temperature 200 °C
0.000127 ohm-cm
@Temperature 392 °F
Bimetal
 0.000133 ohm-cm
@Temperature 300 °C
0.000133 ohm-cm
@Temperature 572 °F
Bimetal
 
Thermal PropertiesMetricEnglishComments
CTE, linear  1.45 µm/m-°C
@Temperature 30.0 - 130 °C
0.806 µin/in-°F
@Temperature 86.0 - 266 °F
 28.1 µm/m-°C
@Temperature 30.0 - 130 °C
15.6 µin/in-°F
@Temperature 86.0 - 266 °F
High-expansive component
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 6.00 W/m-K
@Temperature 20.0 °C
41.6 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 330 °C626 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Descriptive Properties
Linearity Range, °C-20 to 300
linearity Temperature Range, °C-20 to 250
Specific thermal curvature, /K0.000039
Specific deflection, /K0.0000208

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV122 / 19016

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.