MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes:

Applications: Wet corrosion resistance and general service.

Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.

Key Words: EN 1.4311; ASTM 304LN; JIS SUS 304LN
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/ccRT
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 550 MPaEN 10002-1
 640 MPaOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 410 MPa
@Temperature 300 °C
EN min.; EN 10002-5
 430 MPa
@Temperature 200 °C
EN min.; EN 10002-5
 490 MPa
@Temperature 100 °C
EN min.; EN 10002-5
 850 MPa
@Temperature -80.0 °C
EN min; EN 10002-5
 1250 MPa
@Temperature -196 °C
EN min; EN 10002-5
Tensile Strength, Yield 270 MPa
@Strain 0.2 %
EN min., RT; EN 10002-1
 310 MPa
@Strain 1 %
EN min., RT; EN 10002-1
 320 MPa
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 360 MPa
@Strain 1 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 119 MPa
@Strain 0.2 %,
Temperature 500 °C
EN min.; EN 10002-5
 125 MPa
@Strain 0.2 %,
Temperature 400 °C
EN min.; EN 10002-5
 136 MPa
@Strain 0.2 %,
Temperature 300 °C
EN min.; EN 10002-5
 149 MPa
@Strain 1 %,
Temperature 500 °C
EN min.; EN 10002-5
 156 MPa
@Strain 1 %,
Temperature 400 °C
EN min.; EN 10002-5
 157 MPa
@Strain 0.2 %,
Temperature 200 °C
EN min.; EN 10002-5
 167 MPa
@Strain 1 %,
Temperature 300 °C
EN min.; EN 10002-5
 187 MPa
@Strain 1 %,
Temperature 200 °C
EN min.; EN 10002-5
 205 MPa
@Strain 0.2 %,
Temperature 100 °C
EN min.; EN 10002-5
 240 MPa
@Strain 1 %,
Temperature 100 °C
EN min.; EN 10002-5
 350 MPa
@Strain 0.2 %,
Temperature -80.0 °C
EN min.; EN 10002-5
 420 MPa
@Strain 1 %,
Temperature -80.0 °C
EN min.; EN 10002-5
 550 MPa
@Strain 0.2 %,
Temperature -196 °C
EN min.; EN 10002-5
 650 MPa
@Strain 1 %,
Temperature -196 °C
EN min.; EN 10002-5
Elongation at Break >= 40 %EN 10002-1
 55 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 35 %
@Temperature -196 °C
EN min
 40 %
@Temperature -80.0 °C
EN min
Modulus of Elasticity 200 GPaRT
 165 GPa
@Temperature 500 °C
 172 GPa
@Temperature 400 °C
 179 GPa
@Temperature 300 °C
 186 GPa
@Temperature 200 °C
 194 GPa
@Temperature 100 °C
Poissons Ratio 0.30RT
Shear Modulus 77.0 GPacalculated
Impact Test >= 60.0 JHot rolled plate/Cold rolled strip/sheet, 10x10mm test pieces; EN 10045-1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000730 ohm-cmRT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 100 °C
 16.5 µm/m-°C
@Temperature 200 °C
 17.0 µm/m-°C
@Temperature 300 °C
 17.5 µm/m-°C
@Temperature 400 °C
 18.0 µm/m-°C
@Temperature 500 °C
Specific Heat Capacity 0.500 J/g-°CRT
Thermal Conductivity 15.0 W/m-KRT
 20.0 W/m-K
@Temperature 400 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.020 %
Chromium, Cr 18.5 %
Iron, Fe 70.84 %
Nickel, Ni 10.5 %
Nitrogen, N 0.14 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel CLC 18.10 LN Nitrogen Containing 18Cr-10Ni Austenitic Stainless Steel
316 Stainless Steel, annealed sheet
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel
Crucible Steel SUE52 Martensitic Steel
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel

NOUTOK14 / 18729

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.