MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo Domamid® 24 T Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: DOMAMID® 24 T are a low viscous Polyamide 6 pellets produced from Caprolactam by polymerization. Domamid T products are special textile grades with a high uniformity of relative viscosity and Amino-end groups.

Applications:

  • Textile yarn extrusion
  • Compounding
  • Injection moulding
  • Information provided by Domo

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.14 g/cc
    Volatiles <= 0.60 %Extractables; BUP - 06
    Apparent Bulk Density 0.600 - 0.800 g/cc
    Viscosity Measurement 2.42 - 2.48
    @Temperature 20.0 °C
    1% Solution in 96% H2SO4; BUP - 02
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 221 °C
     
    Processing PropertiesOriginal ValueComments
    Moisture Content <= 0.060 %BUP - 05
     
    Descriptive Properties
    Amino-End groups40 ± 2 meq/kg
    Chip Numberca. 100/g

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Domo Domamid® 24 Polyamide 6
    Domo Domamid® 27 Polyamide 6
    Domo Domamid® 24 T-HS Polyamide 6
    Domo Domamid® 33 Polyamide 6
    Domo Domamid® 2403 T-HS Polyamide 6

    PDOMO25 / 30193

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.