MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake Epolene® C-18 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Epolene C-18 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersion, and applications requiring compatibility with polyamide. Coatings produced with Epolene C-18 exhibit high gloss, low moisture vapor transmission rates, grease resistance, and good heat seal ability. In hot melt adhesives, the maleic anhydride modification allows for improved adhesion, greater filler tolerance, broader capabilities, and improved aging properties.
    Key Attributes:
  • Enhances paraffin wax coating properties like gloss, grease resistance, and MVTR
  • Excellent thermal stability
  • Maleic anhydride grafted PE provides functionality
  • Medium molecular weight
  • Useful in color concentrates
    Application/Uses:
  • Automotive OEM
  • Automotive refinish
  • Automotive
  • Building and Construction
  • Hot Melt Adhesives
  • Packaging
  • Solvent borne Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 - 0.920 g/cc
Viscosity 2400 - 6000 cP
@Temperature 150 °C
542-111
Brookfield Viscosity 1550 cP
@Temperature 190 °C
ASTM D3226
 7750 cP
@Temperature 125 °C
ASTM D3226
Molecular Weight 15000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 1.5 - 2.5542-110
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 261 °C
Ring & Ball Softening Point 101 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number >= 1.0542-130
 
Descriptive Properties
Penetration Hardness4 dmmASTM D5, Needle under 100-g load for 5s @ 25°C, tenths of mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Epolene® C-26 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed
Westlake Epolene® C-19 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed
Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
LyondellBasell Plexar® PX2250 Extrudable Tie-Layer Resin, Anhydride Modified HDPE
Westlake Epolene® E-10 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer

PWESF9023 / 106860

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.