MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems DuraForm® FR1200 Flame-retardant nylon 12
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: A flame-retardant nylon 12 material with high accuracy and excellent surface finish. Ideally suited for direct 3D production in aerospace, transportation and consumer goods applications where reliable fire retardancy and reduced smoke and toxicity are required.

Applications:

  • Direct 3D production of aircraft interior parts
  • Parts requiring flame retardancy
  • Automotive and transportion related parts where fire safety may be needed
  • Consumer electronics and other goods
Features:
  • FAR 25.853 compliant
  • Passes AITM smoke density and toxicity requirements
  • High accuracy and repeatability needed for manufacturing
  • Non-halogenated formulation
  • Excellent surface quality
Benefits:
  • Reduce fuel costs with weight optimized design enabled by additive manufacturing
  • Accelerate changes in cabin designs for in service aircraft
  • Eliminate tooling and minimize spare part stocking costs
  • Excellent flame retardancy at 12 and 60 second exposures

Information provided by 3D Systems

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³Sintered Part; ASTM D792
Water Absorption 0.29 %0.29 %ASTM D 570-98
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 41.0 MPa5950 psiASTM D 638
Elongation at Break 5.9 %5.9 %ASTM D 638
Tensile Modulus 2.04 GPa296 ksiASTM D 638
Flexural Strength 62.0 MPa8990 psiUltimate; ASTM D 790
Flexural Modulus 1.77 GPa257 ksiASTM D 790
Izod Impact, Notched 0.250 J/cm
@Thickness 3.05 mm
0.468 ft-lb/in
@Thickness 0.120 in
ASTM D256
Izod Impact, Unnotched 2.33 J/cm
@Thickness 3.05 mm
4.37 ft-lb/in
@Thickness 0.120 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.97e+14 ohm-cm5.97e+14 ohm-cmASTM D257
Surface Resistance 2.56e+13 ohm2.56e+13 ohmASTM D257
Dielectric Constant 3.0
@Frequency 1000 Hz
3.0
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 22.6 kV/mm574 kV/inASTM D149
Dissipation Factor 0.038
@Frequency 1000 Hz
0.038
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 140 µm/m-°C
@Temperature 0.000 - 145 °C
77.8 µin/in-°F
@Temperature 32.0 - 293 °F
ASTM E831
Specific Heat Capacity  1.38 J/g-°C
@Temperature 23.0 °C
0.330 BTU/lb-°F
@Temperature 73.4 °F
ASTM E1269
 1.68 J/g-°C
@Temperature 50.0 °C
0.402 BTU/lb-°F
@Temperature 122 °F
ASTM E1269
 2.03 J/g-°C
@Temperature 100 °C
0.485 BTU/lb-°F
@Temperature 212 °F
ASTM E1269
 2.51 J/g-°C
@Temperature 150 °C
0.600 BTU/lb-°F
@Temperature 302 °F
ASTM E1269
Thermal Conductivity 0.220 W/m-K1.53 BTU-in/hr-ft²-°FASTM E1530
Deflection Temperature at 0.46 MPa (66 psi) 180 °C356 °FASTM D638
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C201 °FASTM D638
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 V-2
@Thickness 5.00 mm
V-2
@Thickness 0.197 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 299 F X 125585 H Nylon 12 (PA); Flame Retardant - Halogen Free
Overview of materials for Nylon 12
3D Systems DuraForm® ProX® FR1200 Flame-retardant nylon 12
EMS-Grivory Grilamid® 1SBVX-30H LDS black PA1010-GF30
Arkema Rilsamid® AECHVO TL PA12

PAPPR3149 / 239117

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.