MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® TP 207 Cation Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® TP 207 is a weakly acidic, macroporous cation exchange resin with chelating iminodiacetat groups for the selective extraction of heavy metal cations from weakly acidic to weakly basic solutions. Divalent cations are removed from neutralized waters in the following order: Copper>Vanadium (VO2)>Uranium (UO2)>Lead>Nickel>Zinc>Cadmium>Iron (II)>Beryllium>Manganese> Calcium>Magnesium>Strontium>Barium>>>Sodium. It is especially suitable for use in the following applications:
  • the selective removal of trace heavy metals from effluents of the metal surface finishing industry, even in the presence of high calcium concentrations
  • the recovery of useful metals from electroplating rinse waters
  • the removal of metal contaminants from processing baths
  • the concentration, extraction and recovery of heavy metals from hydrometallurgical solutions
  • the removal of heavy metals from contaminated ground water for the purpose of potable water production or ground water remediation.
The selective extraction is achieved even in the presence of the following complexing agents:
  • nitrogen compounds, e.g. ammonia, aliphatic and aromatic amines
  • multivalent carboxylic acids, e.g. citric acid, gluconic acid, glucuronic acid, oxalic acid, tartaric acid
  • phosphates, e.g. tetrasodium diphosphate, sodium polyphosphate
Lewatit TP 207 does not remove heavy metals from solutions containing EDTA or NTA respectively. Only cadmium is removed from solutions containing cyanides. For the extraction of those heavy metals which follow the uranyl oxide ion in the selectivity sequence as shown above. Lewatit TP 207 has to be conditioned with caustic soda solution after every regeneration cycle before every exhaustion cycle. After the conditioning it is partially in a salt-form, e.g. mono-sodium-form.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.720 g/cc
Density 1.17 g/cc
Bead Size 0.500 - 0.600 mmMean
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceBeige, opaque
pH Operating Range2 - 9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8846 / 209238

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.