MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SIMONA America SIMONA® 010024378 ECTFE 902
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: Offers exceptional chemical resistance up to 300°F (149°C). FM 4910 limited use approval for thick-walled machined parts and deep draw thermoforming.

Information provided by Simona America Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.71 g/cc1.71 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %ASTM D570
Thickness 50800 microns2000 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7373ASTM D2240
Tensile Strength, Yield 31.0 MPa4500 psiASTM D638
Elongation at Break 255 %255 %ASTM D638
Flexural Modulus 1.69 GPa245 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Coefficient of Friction, Dynamic 0.200.20ASTM C1894
Coefficient of Friction, Static 0.100.10ASTM C1894
Taber Abrasion, mg/1000 Cycles 5.05.0CS 17
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM D696
Melting Point 223 °C434 °FASTM D3418
Maximum Service Temperature, Air 150 °C302 °F
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C195 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C160 °FASTM D648
Flammability, UL94 V-0V-0
 
Descriptive Properties
Colornatural
Length (in)48
Regulatory CodeFM 4910
Width (in)48

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIMONA431 / 285159

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.