MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® 9012 HDPE Injection Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 55600

Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage Resistance

Applications:Food Pails (2-5 gallon), Automotive, Toys, Closures, Housewares

Data provided by Chevron Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D1505
Apparent Bulk Density 0.590 g/ccASTM D1895
Melt Flow 11.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
High Load Melt Index 299 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.5 MPaASTM D638
Elongation at Break 700 %ASTM D638
Flexural Modulus 0.970 GPa3 pt. secant; ASTM D790
 1.24 GPa3 pt. Tangent; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 123 °CASTM D1525
Brittleness Temperature <= -71.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin
Chevron Phillips Marlex® 9006 HDPE Injection Molding Resin
Chevron Phillips Marlex® 9005 HDPE Injection Molding Resin
Renishaw 9012 Vacuum casting resin

PCHEVV40 / 20436

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.