MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® L XE 10953 black PA12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Grilamid L Polyamide 12 (PA12) is formed by the polymerisation of laurolactam, a ring-shaped, long-chain monomer with 12 carbon atoms. It has low water absrorption, excellent hydrolysis resistance, and low density relative to other polyamides.

Data provided by EMS-Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³Dry; ISO 1183
Water Absorption 1.2 %1.2 %Sim. to ISO 62
Moisture Absorption 0.600 %0.600 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.011 cm/cm0.011 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  63
@Time 15.0 sec
63
@Time 0.00417 hour
Dry; ISO 868
 63
@Time 15.0 sec
63
@Time 0.00417 hour
Conditioned; ISO 868
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Conditioned; ISO 527-1/-2
Tensile Modulus 0.400 GPa58.0 ksiConditioned; ISO 527-1/-2
 0.500 GPa72.5 ksiDry; ISO 527-1/-2
50% Modulus  30.0 MPa
@Strain 50 %
30.0 MPa
@Strain 50 %
Dry; ISO 527-1/-2
 30.0 MPa
@Strain 50 %
30.0 MPa
@Strain 50 %
Conditioned; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+6 ohm-cm1.00e+6 ohm-cmDry; IEC 60093
 1.00e+6 ohm-cm1.00e+6 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+6 ohm1.00e+6 ohmIEC 60093
Dielectric Strength 12.0 kV/mm305 kV/inConditioned; IEC 60243-1
 14.0 kV/mm356 kV/inDry; IEC 60243-1
Comparative Tracking Index 150 V150 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 140 µm/m-°C77.8 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°C100 µin/in-°FISO 11359-1/-2
Melting Point 173 °C343 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C194 - 230 °FLong Term; ISO 2578
 150 °C302 °FShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRH056a / 291320

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.