MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco RPM® SAE 75W-90 Synthetic Gear Lubricant
Categories: Fluid; Lubricant

Material Notes: Features

Chevron RPM Synthetic Gear Lubricant is a heavy duty, extreme pressure, multigrade automotive gear lubricant.

It is manufactured from synthesized hydrocarbon base fluids which have excellent thermal and oxidation stability, a high viscosity index, and a low pour point. The low pour point of Chevron RPM Synthetic Gear Lubricant imparts improved lubrication during startup at subzero temperatures, while the improved viscositytemperature characteristics provide dependable lubrication at high temperatures. Lower frictional losses in the lubricant film and reduced churning losses due to lower bulk oil viscosity lead to reduced operating temperatures when compared to conventional gear lubricants.

Applications

Chevron RPM Synthetic Gear Lubricant is recommended as a rear axle and differential lubricant in over-the-road and off-road vehicles when operating under severe conditions and in extremely cold or hot environments.

Chevron RPM Synthetic Gear Lubricant meets or exceeds the requirements of API Service Categories GL-4, GL-5 and MT-1. In addition, it is approved for:

  • Dana Corporation, Spicer Axle Division SHAES 256
  • Eaton Corporation E500 PS-163
  • Mack GO-J
  • Meritor O-76N Extended Drain
  • SAE J2360 (formerly MIL-PRF-2105E)
These approvals allow the use of Chevron RPM Synthetic Gear Lubricant in Dana, Eaton, and Meritor axles with 500,000-mile drain intervals and 750,000-mile extended equipment warranty.

Key Words: CPS Number: 210457; MSDS Number: 4895
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 29.8 °
Viscosity Measurement 150Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 611 SUS
Saybolt Viscosity at 210°F 86.6 SUS
Kinematic Viscosity at 40°C (104°F) 117 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15.5 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -48.0 °CASTM D97
Flash Point 204 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco TEGRA® SAE 75W-90 Synthetic Gear Lubricant
ExxonMobil Mobil Delvac 75W-90 Synthetic Gear Oil
Phillips 66 MP Gear Lube SAE Grade 75W-90
Phillips 66 Inca® 1000 Oil, AGMA No. 8A Comp.
Phillips 66 680 Bearing Oil

WCHEV218 / 74833

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.