MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Coating P. Materials EB-90AO TPU for Film and Sheet
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: CPMC produces and specializes on TPU materials for film and sheet use, which is widely processing in common use and increase working efficiency. TPU apply to film and sheet with good characteristics including as below,+ Process easily+ Endurance at low temperature and maturing)

Product Description: Water vapor permeability type, excellent water resistance, nice touch, good physical properties and elasticity. Good fluidity, well controlled viscosity, good workability etc.

Application To End-Use Products: Shoe products, clothes, medical supplies, industrial goods and baby products

Information provided by Coating P. Materials Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 88 - 9288 - 92ASTM D2240
Tensile Strength 39.2 MPa5690 psiASTM D412
Elongation, Ultimate 700 %700 %ASTM D412
100% Modulus 9.32 MPa1350 psiASTM D412
300% Modulus 22.6 MPa3270 psiASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTCOAT025 / 293969

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.