MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Crosspolimeri POLIGOM G/7 CPR EPR/HEPR/EPDM
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: POLIGOM: is the trade-mark of our crosslinkable EPR/HEPR/EPDM.

POLIGOM G/7 CPR: halogen free chemically crosslinkable elastomer for low voltage cable insulation and sheathing: suitable for G7.It is a conveniently grafted compound able to react in presence of moisture and of a catalyst. We normally suggest our catalyst type MAC/100 SCU or MAC/203 (less reactive type). FOR SOLAR CABLES INSULATION WE SUGGEST TO USE CATALYST MAC/400 PS or MAC/520 PSL (less reactive); both at 7/10%. REACTION BETWEEN GRAFTING AND CATALYST: These two compounds, separately stored, must be mixed before starting extrusion in the ratio: GRAFTING/CATALYST 95/5

Certify: EN 50363-0 G7, BS 7655 GP4-GP5-GP6-GP7, HD 22.1 EI7

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.990 g/ccASTM D792
Melt Flow 2.0 - 6.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ASTM D2240
Tensile Strength >= 13.0 MPaIEC 60811
 >= 13.52 MPa
@Temperature 127 °C,
Time 144000 sec
Air bomb; IEC 60811
 >= 13.91 MPa
@Temperature 150 °C,
Time 605000 sec
Heat Ageing; IEC 60811
Elongation at Break >= 250 %IEC 60811
 >= 225 %
@Temperature 150 °C,
Time 605000 sec
Heat Ageing; IEC 60811
 >= 257.5 %
@Temperature 127 °C,
Time 144000 sec
Air bomb; IEC 60811
Tensile Modulus 7.10 MPaIEC 60811
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 4.00e+15 ohm-cmIEC 60502
Dielectric Strength 39.0 kV/mmASTM D149
 
Processing PropertiesOriginal ValueComments
Zone 1 140 °C
Zone 2 160 °C
Zone 3 180 °C
Zone 4 190 °C
Die Temperature 205 °C
Head Temperature 190 °C
 
Descriptive Properties
Hot Set Test0Residual Value, IEC 811
 0.6250°C - 20 N/cm2, IEC 811

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS135 / 294219

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.