MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lanxess LEWATIT® S 4528 Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® S 4528 is a food grade, macroporous, heterodisperse, weakly basic anion exchange resin based on a styrene-divinylbenzene copolymer. It is bead-shaped and has a special bead size distribution for use in the following processes:
  • Lewatit WS system (fluidized bed)
  • Lewatit VWS system (compound fluidized bed)
  • Standard co current regenerated system.
Lewatit S 4528 is suitable in the free base for the removal of acid and simultaneous decolorization of solutions of organic products such as sugar, gelatin, glycerin, grape must, whey, fruit concentrates, etc. The macroporous structure ensures very good adsorption of both acid and organic substances (e.g. colorants). These are desorbed by regeneration with caustic soda solution. Due to its low basicity, Lewatit S 4528 can be used in the treatment of products sensitive to alkali. The partial isomerization resulting from contact with the ion exchange resin (e.g. conversion of glucose to fructose and mannose) is negligible. If using the Lewatit S 4528 to treat potable water and the aqueous solution listed above, special care should be given to the initial cycles of the new resin.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.620 g/cc0.0224 lb/in³
Density 1.02 g/cc0.0368 lb/in³
Bead Size 0.400 - 1.25 mm0.0157 - 0.0492 in>90%
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceBeige, opaque
pH Operating Range0 - 8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8828 / 209220

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.