MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical LUMID HI5006A(W) PA6/ABS, High Impact, Good Dimensional Stability
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Feature: Injection Molding, PA6/ABS, High Impact, Good Dimensional Stability

Application: Pipe Fitting, Electrical and Electronic parts

CAS No. 25038-54-4, 9003-56-9 and 9003-54-7

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Water Absorption 0.70 %ASTM D570
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 450 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 100 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 600 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Flexural Modulus 16000 kg(f)/cm²
@Thickness 3.20 mm
1.3mm/min; ASTM D790
Izod Impact, Notched 70.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 2.9
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 26.0 kV/mm
@Thickness 1.00 mm
ASTM D419
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°CASTM D696
Melting Point 220 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 235 - 250 °CInjection Molding
Middle Barrel Temperature 240 - 260 °CInjection Molding
Front Barrel Temperature 240 - 260 °CInjection Molding
Nozzle Temperature 250 - 265 °CInjection Molding
Melt Temperature 250 - 265 °CInjection Molding
Mold Temperature 80.0 - 100 °CInjection Molding
Drying Temperature 70.0 - 90.0 °CInjection Molding
Dry Time 4.00 - 5.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUMID HM2604AW PA6+GF60%
LG Chemical LUMID GP3400A(W) PA6+MF40%, General Purpose
LG Chemical LUMID HI3232A(W) PA6+MF23%, High Impact
LG Chemical LUMID HI1102A(W) PA6, High Impact
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact

PLAY165 / 148175

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.