MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lendell Manufacturing SRF-1 Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes:

This line of foam is formulated specially for slow recovery or "memory" effects. Once the foam is physically contacted, the foam retains the shape of the contacting object for a brief period of time. The duration of this period can varied from seconds to minutes, depending on the form of Visco.

Applications:

Shock Absorption, Soft-Foam Earplugs, Fruit and Vegetable Drying Sponges, Shoe Insoles, Visco Foam Squeeze Balls, Molded Toys and Ad Specialty Items, Earwarmers, Mattresses-Pillows, Lumbar Supports, and Wheelchair Pads

Information provided by Lendell Manufacturing Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.92 lb/ft³Core
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 23.7 psiASTM D3574
Elongation at Yield 408.9 %
Tear Strength 1.85 pli
 5.30 pliDie "C", average; ASTM D3574
Compression Set 40.6 %50%; Humid Aged
 42.9 %50%; Original
 71.9 %75%; Humid Aged
 73.3 %75%; Original
 
Descriptive Properties
Air Flow Rate, cfm0
Ball Rebound, %5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Struktol STRUKSILON 8104 Silicone Stabilizer for PU Foam
American Red Oak Wood
3M RPF-C (0.32 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
3M RPF-C (0.24 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass
General Plastics LAST-A-FOAM® R-9320 Thermal Isolation Blocks

PLEND05 / 50780

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.