MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC VALOX™ 745 PBT (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: 30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.44 g/ccASTM D792
 1.46 g/ccASTM D792
Water Absorption 0.090 %24 hours; ASTM D570
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
@Thickness 1.50 - 3.20 mm
SABIC method
 0.0080 - 0.010 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Thickness 1.50 - 3.20 mm
SABIC method
 0.0080 - 0.010 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 112ASTM D785
Tensile Strength at Break 46.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 48.0 MPa50 mm/min; ASTM D638
Flexural Yield Strength 89.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3440 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 80.0 J/mASTM D256
Izod Impact, Unnotched 1602 J/mASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.90e+16 ohm-cmASTM D257
Dielectric Constant 3.2
@Frequency 1e+6 Hz
ASTM D150
 3.3
@Frequency 100 Hz
ASTM D150
Dielectric Strength 23.2 kV/mm
@Thickness 3.20 mm
in air; ASTM D149
 24.8 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
Dissipation Factor 0.0020
@Frequency 100 Hz
ASTM D150
 0.014
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI 30 - 60 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 75.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 139 µm/m-°C
@Temperature 60.0 - 138 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 HB
@Thickness 1.47 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 255 - 270 °CInjection Molding
Zone 1 245 - 255 °C
Zone 2 250 - 260 °C
Zone 3 255 - 265 °C
Melt Temperature 255 - 275 °C
Mold Temperature 65.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 12.0 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 80 %
Vent Depth 0.00250 - 0.00380 cm
Screw Speed 50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10238 / 243705

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.