MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Colorite Polymers 6534 General Purpose Vinyl Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame retardance, low temperature, or chemical resistance, are all available. Formulations for exterior or interior use.

Typical Applications: Clear General Purpose Molding

Information provided by Colorite Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 6510 sec; ASTM D2240
Tensile Strength, Ultimate 1670 psiASTM D638
Elongation at Break 440 %ASTM D638
100% Modulus 0.620 ksi
@Strain 100 %
ASTM D638

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PVC, Molded
Sibur VO Compound VNP Polyvinyl Chloride (PVC)
Overview of materials for PVC, Wire and Cable Grade
CoreLite PVC 60 Closed-Cell PVC Foam Sheet
Colorite Polymers Self Frosting™ 7011SF Vinyl Compound

PCOL190 / 28909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.