MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) KetaSpire® XT-920 GF30 PEEK, 30% glass fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: KetaSpire® XT-920 GF30 is a 30% glass fiber reinforced, natural color grade of the industry's first true a high-temperature PEEK. Glass fiber reinforcement provides higher strength and stiffness properties than unreinforced KetaSpire® XT-920 resin, making it suitable for structural applications needing robust mechanical properties, particularly those with service temperatures approaching 300°C.

The PEEK designation is based on the 2:1 ratio of ether-to-ketone functional groups in the polymer backbone. The material provides the exceptional chemical resistance of PEEK along with a 20°C (36°F) higher glass transition temperature and a 45°C (81°F) higher melting temperature than standard PEEK. This increase in thermal performance allows engineers to achieve higher mechanical strength for components used in higher temperature and higher pressure operating environments.

Although other high-temperature polyketones exhibit thermal properties on par with KetaSpire® XT, their chemical resistance is significantly inferior to standard PEEK and KetaSpire® XT. The material's unique combination of properties makes KetaSpire® XT well-suited for applications in oil & gas, transportation, electronics, chemical processing, and other industrial uses.

Applications: Aircraft Applications; Automotive Applications; Connectors; Electrical/Electronic Applications; Housings; Industrial Applications; Oil/Gas Applications; Pump Parts; Seals

Features: Chemical Resistant; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Impact Resistance; High Heat Resistance; Radiotranslucent; Steam Resistant

Information provided by Solvay Specialty Polymers.

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccASTM D792
Viscosity 670 cP
@Shear Rate 1000 1/s,
Temperature 420 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 2.00 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm
@Thickness 2.00 mm
ASTM D955
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 420 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 101ASTM D785
Hardness, Shore D 87
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 156 MPa5.0 mm/min; ASTM D638
 165 MPaType 1A, 5 mm/min; ISO 527-2
Elongation at Break 3.0 %ISO 527-2
 3.0 %5.0 mm/min; ASTM D638
Tensile Modulus 10400 MPa5.0 mm/min; ASTM D638
 10700 MPaType 1A; ISO 527-2
Flexural Strength 243 MPaASTM D790
 258 MPaISO 178
Flexural Modulus 9900 MPaASTM D790
 10300 MPaISO 178
Compressive Strength 166 MPaASTM D695
Shear Strength 91.0 MPaASTM D732
Izod Impact, Notched 110 J/mASTM D256
Izod Impact, Unnotched 950 J/mASTM D256
Izod Impact, Notched (ISO) 12.0 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 56.0 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.33
@Frequency 1e+6 Hz
ASTM D150
 3.37
@Frequency 1000 Hz
ASTM D150
 3.38
@Frequency 60 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm
@Thickness 1.60 mm
ASTM D149
Dissipation Factor 0.0010
@Frequency 1000 Hz
ASTM D150
 0.0010
@Frequency 60 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 17.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
Melting Point 385 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 332 °CAnnealed; ASTM D648
Glass Transition Temp, Tg 170 °CDSC
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 405 °C
Middle Barrel Temperature 405 °C
Front Barrel Temperature 410 °C
Nozzle Temperature 410 °C
Mold Temperature 205 - 230 °C
Drying Temperature 150 °C
@Time 14400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ColorBeige
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
RoHS ComplianceYes
Screw Compression Ratio2.5:1.0 to 3.5:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4354 / 280154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.