MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Lehvoss LUVOCOM® 1800-9333/WT PET unreinforced, thermally conductive modified  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Properties/attributes include: Strong, stiff parts. Heat stabilized. Isotropic shrinkage characteristics.

Automotive industry, textile- and office machinery, apparatus- and precision engineering. Typical uses include: Parts for electric and electronic industry.

Processing: During processing the moisture level should not exceed 0.02%, otherwise molecular degradation and surface defects (e.g. smearing) may occur. As the material absorbs water very quickly, the predried material should be fed to the processing immediately. Processing temperatures above 300°C may very rapidly cause thermal damage and should therefore be avoided. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccISO 1183
Moisture Absorption <= 0.300 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.300 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 54.0 MPa7830 psiISO 527-2
Elongation at Break 1.1 %1.1 %ISO 527-2
Modulus of Elasticity 9.50 GPa1380 ksiISO 527-2
Flexural Strength 85.0 MPa12300 psiISO 178
Flexural Modulus 8.50 GPa1230 ksiISO 178
Flexural Strain at Break 1.8 %1.8 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 2.20 J/cm²
@Temperature 23.0 °C
10.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eU
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60167
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C16.7 µin/in-°FDIN 53752
Thermal Conductivity 7.00 W/m-K48.6 BTU-in/hr-ft²-°F|| 60x60x3 mm; HOT-DISK
Maximum Service Temperature, Air 100 °C212 °FContinuous; UL 746B
 180 °C356 °FShort Term
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 265 - 275 °C509 - 527 °F
Zone 1 285 - 295 °C545 - 563 °F
Zone 2 270 - 280 °C518 - 536 °F
Zone 3 265 - 275 °C509 - 527 °F
Melt Temperature 280 °C536 °F
Mold Temperature 60.0 - 120 °C140 - 248 °F
Drying Temperature  80.0 °C
@Time 21600 - 28800 sec
176 °F
@Time 6.00 - 8.00 hour
 120 °C
@Time 7200 - 18000 sec
248 °F
@Time 2.00 - 5.00 hour
Dehumidifying dryer
Moisture Content <= 0.020 %<= 0.020 %
 
Descriptive Properties
Colorwhite

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 1301-7896 PPS, linear with carbon fiber, thermally conductive modified
LATI Laticonther 62 GR/70 PA 6, 70% Graphite Reinforced
Lehvoss LUVOCOM® 1/CF/40 Polyamide 66 with carbon fiber, heat stabilized
Avient Therma-Tech™ PI-5000 TC Polyetherimide (PEI)
Sumitomo Bakelite Sumikon® FM-XTK-310 Polyphenylene sulfide

PLUU8888 / 193847

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.